Pure Resin Co., Ltd.

Pure Resin Co., Ltd.

Latest information at the first time!

Products
Hydrometallurgical Resin
Hydrometallurgical Resin
Pure Type Ionic Form Moisture
(%)
Vol. Cap.
(mmol/ml)
S/W (g/ml) Particle Size
(%)
Comments
PU1001 Strong Base

Cl-

48-58 ≥1.3 0.66-0.71 0.315-1.40mm≥95 Extraction and separation of tungsten, molybdenum and gold in hydrometallurgy. Extraction of uranium
PU2000 Macroporous Type Strong Base

Cl-

50-60 ≥1.15 0.66-0.76 0.63-1.40mm≥95 Adsorption and purification of uranium in uranium ores, enrichment and separation of thorium, plutonium and uranium in the nuclear industry, treatment and recovery of vanadium in ammonia production wastewater, separation and removal of zinc in nickel electrolyte
PU2000-Ⅱ Macroporous Type Strong Base

Cl-

40-50 ≥3.2 0.66-0.75 0.63-1.40mm≥95 It adsorbs and purifies uranium in uranium ores, enriches and separates thorium, plutonium and uranium in the nuclear industry, and separates and purifies vanadium in hydrometallurgy.
PU2001 Macroporous Type Strong Base Type Ⅱ

Cl-

47-57 ≥1.15 0.68-0.76 0.315-1.40mm≥95 It is specially used for concentrated hydrochloric acid iron removal and purification treatment, and has the characteristics of high iron removal rate and high water elution rate
PU3100 Macroporous Type Weak Base

Free Base

43-46 ≥1.3 0.66–0.70 0.60-1.20mm≥95 It is used for selective adsorption and efficient recovery of rhenium from hydrometallurgical leach solutions
PU3000-Au Macroporous Type Weak Base

Free Base

50-60 ≥1.4 0.65-0.73 0.71-1.40mm≥95 It is specially designed for the adsorption and recovery of gold in hydrometallurgical gold solutions and wastewater, and has excellent osmotic strength and dynamic properties
PU3000M Macroporous Type Weak Base

Free Base

50-60 ≥1.4 0.66-0.73 0.315-1.40mm≥95 It is specially used for the separation and purification of molybdenum in hydrometallurgy
PU3000-v Macroporous Type Weak Base

Free Base

50-60 ≥1.4 0.66-0.73 0.315-1.40mm≥95 It is used in hydrometallurgy, the purification of vanadium and molybdenum
PU3000 Macroporous Type Weak Base Free Base 50-60 ≥1.4 0.65-0.73 0.315-1.40mm≥95 Adsorption and recovery of hexavalent chromium in chromium-containing solutions
PU5011 Acrylic-based Macroporous Type Weak Base

Free Base

50-60 ≥2.6 0.65-0.75 0.45-1.40mm≥95 It is used to separate and remove lead in nickel or cobalt electrolytes, and vanadium in molybdate solutions
PU400MV Macroporous Type Imidediacetic Acid Chelating Resin

Na+

40-50 ≥1.0 0.71-0.75 0.45-1.40mm≥95 It is used in hydrometallurgy, the purification of vanadium and molybdenum

The last letters are all metal ions